AWS ERNiCrMo-7 Nickel Alloy Welding Wire Mig and Tig Wire, Arc Welding Rods Best Welding Supplier

Short Description:

ERNiCrMo-10 is used for welding nickel-chromium-molybdenum base materials to themselves, steel and other nickel base alloys, and for cladding steels. Can be used to weld duplex, super duplex stainless steels.


Product Detail

Product Tags

PRODUCT DESCRIPTION:

AWS: A5.14

Conforms to Certification: AWS A5.14                ASME SFA A5.14

Weld Process: GMAW & ASAW Welding Processes

ERNiCrMo-10 is used for welding nickel-chromium-molybdenum base materials to themselves, steel and other nickel base alloys, and for cladding steels. Can be used to weld duplex, super duplex stainless steels.

AWS Chemical Composition Requirements

C = 0.015 max Cu = 0.50 max
Mn = 1.0 max Ni = Remainder
Fe = 3.0 max Co = 2.0 max
P = 0.04 max Cr = 14.0 - 18.0
S = 0.03 max Mo = 14.0 - 18.0
Si = 0.08 max W = 0.50 max
Other = 0.50 max Ti = 0.70 max

PLEASE CALL FOR MORE INFORMATION AND AVAILABLE SIZES:

Application

ERNiCrMo-7 is used for welding nickel-chromium-molybdenum base materials to itself, steel and other nickel base alloys and for cladding steel with NI-CR-MO weld material

PRODUCT PARAMETERS:

Deposited Chemcial Composition % (Typical)
C = 0.01 Cr = 16.5 Ni = Balance
Fe = 2.20 Mo = 15.75
Deposited All Weld Metal Properties % (AW)
Tensile Strength 113,00 psi
Elongation 29%

DEPOSITED CHARPY-V-NOTCH IMPACT PROPERTIES:

Not applicable

Recommended Welding Parameters for MIG and SAW Welding of Nickel Alloys
Process Diameter of Wire Voltage (V) Amperage (A) Gas
MIG .035 inches 26 - 29 150 - 190 75 % Argon +25% Helium
.045 inches 28 - 32 180 - 220 75 % Argon +25% Helium
1/16 inches 29 - 33 200 - 250 75 % Argon +25% Helium
SAW 3/32 inches 28 - 30 270 - 350 Suitable Flux May Be Used.
1/8 inches 29 - 32 350 - 450 Suitable Flux May Be Used.
5/32 inches 30 - 33 400 - 550 Suitable Flux May Be Used.