Hardfacing Welding Electrode DIN 8555 (E9-UM-250-KR) Surfacing Welding Electrode, Stick Welding Rods

Short Description:

DIN 8555  (E9-UM-250-KR) is Special electrode with optimal welding and mechanical properties. Austenite- Ferrites weld metal. High strength values and high crack resistance.


Product Detail

Product Tags

Hardfacing Welding Electrode

Standard: DIN 8555  (E9-UM-250-KR)

Type No.: TY-C65

 

Specification&Application:   

· Special electrode with optimal welding and mechanical properties.

· Austenite- Ferrites weld metal. High strength values and high crack resistance.

· Particularly suitable for joining on hardly weldable steels, when highest demands on the welding seam are made.

· High crack resistance when joining parent metals of difficult weldability, such as austenitic and ferritic steels, high-manganese steels with alloyed and non-alloyed steels, heat-treatable and tool steels. Applications in the repair and maintenance of machine and drive components as well as in tool repairing.

· As cushion layer on these materials is also ideally suited.

 

 

Chemical composition of deposited metal(%):            

 

C

Si

Mn

P

S

Cr

Ni

Mo

N

Fe

DIN

-

0.15

-

0.90

 0.50

 2.50

-

0.04

-

0.03

28.0

32.0

8.0

10.0

-

-

Bal.

Typical

0.1

1.0

1.0

≤0.035

≤0.025

29.0

9.0

≤0.75

0.10

Bal.

 

Hardness of deposited metal:

Yield strength

Mpa

Tensile strength

Mpa

Elongation

A(%)

Hardness As Welded

(HB)

620

800

22

240

 

General Characteristics:   

· Microstructure      Austenite + Ferrite

· Machinability        Excellent

· Preheating           Preheating of thick-walled ferritic parts to 150-150℃

· Redrying              Redry for 2 h at 150-200℃ before using.

 

 