AWS E6013 (J421X) Carbon Steel Welding Electrode for Vertical Welding

Short Description:

J421X (AWS E6013) is a high-titanium-potassium-coated electrode for carbon steel welding applications.


Product Detail

Product Tags

Carbon Steel Welding Electrode

J421X                                                         

GB/T E4313

AWS A5.1 E6013                                    

Description: J421X is a high-titanium-potassium-coated electrode for carbon steel welding applications. It can operate in a vertical-down position, and suitable for all-position welding with excellent welding performances, and can be used for both AC and DC. The weld is smooth and neat. The arc is stable and easy to re-strike, slag can be easily removed.

 Application: It applies to welding ship carbon steel and galvanized steel plate as well, in particular, applies welding of the thin plate in a vertical-down position and discontinuous welding application.

 

Chemical composition of weld metal(%):

C

Mn

Si

S

P

≈0.08

≈0.5

≈0.25

≤0.035

≤0.040

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Yield strength

Mpa

Elongation

%

Impact value (J)

Normal Temp.

 0℃

Guaranteed

≥420

≥330

≥17

—

—

Tested

460 ~ 540

370 ~ 420

≈25

≈80

≈70

 X-ray inspection:  II grade

 

Recommended current:

Rod diameter

(mm)

2.0

2.5

3.2

4.0

5.0

Welding current

(A)

50 ~ 70

60 ~ 100

80 ~ 150

160 ~ 200

180 ~ 250

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 