AF2209-16 (AWS E2209-16) is an ultra-low carbon nitrogen-containing duplex stainless steel electrode with titanium-calcium coating.


Product Detail

Product Tags

Stainless Steel Welding Electrode

AF2209-16                               

GB/T E2209-16

AWS A5.4 E2209-16

Description:AF2209-16 is an ultra-low carbon nitrogen-containing duplex stainless steel electrode with titanium-calcium coating. It can be used for both AC and DC with excellent operating performance. Because it contains molybdenum and nitrogen, and the carbon content is extremely low, the deposited metal has good crack resistance and corrosion resistance, especially stress corrosion resistance. 

Application: It is mainly used for welding the same type of ultra-low carbon stainless steel materials in petroleum and hydraulic industries. Such as the welding of 022Cr22Ni5Mo3N duplex stainless steel.

 

Chemical composition of weld metal(%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5 ~ 3.5

0.08 ~ 0.20

≤0.75

≤0.030

≤0.040

 

 Mechanical properties of weld metal:

Test item

 Tensile strength

Mpa

Elongation

%

Guaranteed

≥690

≥20

 

 Recommended current:

Rod diameter

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~70

80 ~ 110

130 ~ 150

160 ~ 200

 

Notice:

1. The electrode must be baked for 1 hour at around 250℃ before welding operation;

2. It is essential to clean up rusty, oil scale, water, and impurities on welding parts before welding.

 

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 