Hardfacing Welding Electrode DIN 8555 (E7-UM-250-KPR) Surfacing Welding Rods, Arc Welding Stick

Short Description:

DIN 8555 (E7-UM-250-KPR) is a Basic coated high recovery SMAW electrode.  Full austenite structure. Very high workhardening and high toughness.


Product Detail

Product Tags

Hardfacing Welding Electrode

 

Standard: DIN 8555 (E7-UM-250-KPR)

Type No.: TY-C BMC

 

Specification & Application:

· Basic coated high recovery SMAW electrode

· Full austenite structure. Very high workhardening and high toughness.

· It is suitable for claddings on parts subject to highest pressure and shock in combination with abrasion. Surfacing can be made on ferritic steel as well as austenitic hard Mn-steel and joints of hard Mn-steel can be welded.

· Main application fields are in the mining and cement industry, railway crossing, dredge pumps, hydraulic press pistons, crusher part undergoing high impact by soft mineral.

 

Chemical composition of deposited metal(%):            

 

C

Si

Mn

Cr

Ni

Mo

V

Fe

DIN

0.5

-

-

11.0

18.0

-

-

3.0

-

-

Bal.

EN

0.3

1.2

-

11.0

18.0

-

19.0

-

3.0

-

2.0

-

1.0

Bal.

Typical

0.6

0.8

16.5

13.5

-

-

-

Bal.

 

 

Hardness of deposited metal:

As Welded

(HB)

Work-hardened

(HB)

260

550

 

General characteristics:

· Microstructure      Austenite

· Machinability       Grinding only

· Interpass temp.     ≤250℃

· Redrying           Redry for 2 h at 300℃ before using.


  • Previous: