E71T-11 A5.20, CARBON STEEL Flux Cored Arc Welding Electrodes
| E71T-11 is a self-shielding flux cored wire used for welding carbon steels. Does not require a shielding gas and can be used in limited multi-pass welding operations.
Typical Applications: butt, lap and fillet welds on steel 16 gauge through ½”; assembly and maintenance welding; machine parts, tanks, prefab construction
| AWS Class: E71T-11 |
Certification: AWS A5.20/A5.20M:2005 |
| Alloy: E71T-11 |
AWS/ASME SFA A5.20 |
Welding Position:
H, F, V-up, O |
Current:
DCEN |
| Tensile Strength, kpsi: |
70-95 |
| Yield Strength, kpsi: |
58 min |
| Elongation %: |
20 min |
Typical Wire Chemistry as per AWS A5.9 (single values are maximum)
| C |
Mn |
Si |
S |
P |
Al |
|
| 0.30 |
1.75 |
0.60 |
0.03 |
0.03 |
1.80 |
|
| |
Typical Wire Parameters |
| Diameter |
Position |
Process |
Amps |
Volts |
Wire Feed Speed |
| in |
(mm) |
|
| .030″ |
0.8 |
All Position |
FCAW |
25 |
14 |
55 |
| |
|
All Position |
FCAW |
125 |
16 |
225 |
| .035″ |
0.9 |
All Position |
FCAW |
55 |
17 |
75 |
| |
|
All Position |
FCAW |
80 |
19 |
110 |
| |
|
All Position |
FCAW |
120 |
20 |
160 |
| .045″ |
1.2 |
All Position |
FCAW |
115 |
15 |
105 |
| |
|
All Position |
FCAW |
130 |
16 |
125 |
| |
|
All Position |
FCAW |
160 |
17 |
170 |
| |
|
All Position |
FCAW |
200 |
18 |
195 |
| 1/6″ |
1.6 |
All Position |
FCAW |
160 |
17 |
70 |
| |
|
All Position |
FCAW |
190 |
18 |
100 |
| |
|
Flat & Horizontal |
FCAW |
210 |
19 |
110 |
| |
|
Flat & Horizontal |
FCAW |
260 |
20 |
145 |
| 0.068 |
1.7 |
All Position |
FCAW |
145 |
18 |
50 |
| |
|
All Position |
FCAW |
155 |
18 |
60 |
| |
|
All Position |
FCAW |
185 |
18 |
70 |
| |
|
All Position |
FCAW |
240 |
18 |
100 |
| |
|
Flat & Horizontal |
FCAW |
255 |
21 |
111 |
| |
|
Flat & Horizontal |
FCAW |
315 |
22 |
160 |
| 5/64 |
2.0 |
All Position |
FCAW |
185 |
16 |
55 |
| |
|
All Position |
FCAW |
190 |
18 |
60 |
| |
|
All Position |
FCAW |
220 |
19 |
70 |
| |
|
Flat & Horizontal |
FCAW |
26 |
21 |
90 |
| |
|
Flat & Horizontal |
FCAW |
315 |
22 |
124
|
|
Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.
Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.
Previous:
AWS: E81T1-Ni1C-JH4, E81T1-C1A4-Ni1-H4 Flux-cored Welding Wire
Next:
Nickel Alloy Welding Wire ERNiCrMo-3 Mig Welding Wire