E316HT1-1 Stainless steel flux cored wire

Short Description:

It has excellent welding process performance such as stable arc, less spatter, good slag removal, stable wire feeding, and beautiful shape


Product Detail

Product Tags

E316HT1-1 Stainless steel flux cored wire 

Product Description
Compliant with the standard: GB/T17853 E316T1-1
AWS A5.22 E316HT1-1

Features and Uses
1. Because it contains a certain amount of carbon, it is suitable for welding high temperature resistant stainless steel equipment;
2. It has excellent welding process performance such as stable arc, less spatter, good slag removal, stable wire feeding, and beautiful shape;
3. Due to the high content of Mo , the corrosion resistance is strong;
4. Suitable for 18%Cr-12%Ni-2%Mo welding in petrochemical, pressure vessel, medical and food machinery, fertilizer and other industries .

Chemical composition (wt%)

Alloy wt% C Mn And Cr In Mo P S With
GB/T 0.08 0.5-2.5 1.0 17.0-22.0 11.0-14.0 2.0-3.0 0.040 0.030 0.50
AWS 0.04-0.08 0.5-2.5 1.0 17.0-22.0 11.0-14.0 2.0-3.0 0.040 0.030 0.75
Example value 0.50 1.45 0.50 18.05 12.00 2.35 0.020 0.005 0.05

 
Mechanical behavior

Mechanical behavior Yield strength MPa Tensile strength MPa  Elongation% Impact value J/℃
GB/T - 520  30 -
AWS - 520 30 -
Example value - 560 35 -

 
Recommended current range: (DC+)

Welding wire diameter (mm) 1.2 1.6
Voltage (V) 22-36 26-38
Current (A) 120-260 200-300
Dry elongation (mm) 15-20 18-25
Gas flow (l/min) 15-25 15-25

 
Welding Precautions
1. Use CO2 protective gas with a purity of ≥99.98% and a gas flow of 20-25L/min .
2. Inter-channel temperature: 16~100 ℃ .
3. When welding, it is necessary to shield from the wind to prevent welding defects from scattering of the shielding gas. Oil, water, etc. at the welding place must be removed.
4. Use up the welding wire as soon as possible after opening the package. If it is not used up, take moisture-proof measures.

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.