Nickel Alloy Welding Wire ERNiCrMo-3 Mig Welding Wire

Short Description:

ERNiCrMo-3 is a high nickel alloy wire developed for welding and cladding nickel-based alloys such as 625 or similar material.


Product Detail

Product Tags

Nickel Alloy Welding Wire ERNiCrMo-3

 

Standards

EN ISO 18274 – Ni 6625 – NiCr22Mo9Nb

AWS A5.14 – ER NiCrMo-3

 

Features and Applications

High nickel alloy wire developed for welding and cladding nickel-based alloys such as 625 or similar material.

Solid drawn in a very special way to obtain cleaner and higher quality welds with a bright seam and excellent ductility.

The weld metal has very good mechanical properties at high and low temperatures.

Good resistance to pitting and stress corrosion.

Recommended working temperature ranges from cryogenic to 540°C.

Precision layer wound for superior wire feeding characteristics.

Typically used in the chemical process industry, marine engineering, nuclear reactor components, aerospace and within pollution control equipment etc.

 

Typical Base Materials

Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926* * Illustrative, not exhaustive list

 

Chemical Composition %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

max

max

max

max

max

max

max

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

max

max

max

20.00

3.15

8.00

Min

1.0

0.40

0.40

23.00

4.15

10.00

 

Mechanical Properties

Tensile Strength

≥760 MPa

Yield Strength

≥415 MPa

Elongation

≥35%

Impact Strength

≥100 J

Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.

Shielding Gases

EN ISO 14175 – I1, I3

Welding Positions

EN ISO 6947 – PA, PB, PC, PD, PE, PF

Packaging Data

Diameter

Weight

Spool

Pallet Qty

1.00 mm

1.20 mm

15 Kg

15 Kg

BS300

BS300

72

72