Nickel Alloy Welding Wire ERNiCr-3 Mig Welding Wire

Short Description:

ERNiCr-3  is used for the welding of alloys 600, 601, 690, 800 and 800HT etc.


Product Detail

Product Tags

Nickel Alloy Welding Wire ERNiCr-3

Standards
EN ISO 18274 – Ni 6082 – NiCr20Mn3Nb
AWS A5.14 – ER NiCr-3

 

Features and Applications

Alloy 82 is used for the welding of alloys 600, 601, 690, 800 and 800HT etc.

Weld metal deposited has high strength and good corrosion resistance, including oxidation resistance and creep rupture strength at elevated temperatures.

Ideal for dissimilar welding applications between various nickel alloys, stainless steels, carbon steels including overlay.

Suitable for applications ranging from cryogenic to high temperatures making this alloy one of the most used in the nickel family.

Precision layer wound for superior wire feeding characteristics.

Typically used in the power generation and petrochemical industries etc.

Typical Base Materials

Alloy 600, Alloy 601, Alloy 690, Alloy 800, Alloy 330*
* Illustrative, not exhaustive list

 

Chemical Composition %

C%

Mn%

Fe%

P%

S%

Si%

max

2.50

max

max

max

max

0.05

3.50

3.00

0.030

0.015

0.50

Cu%

Ni%

Co%

Ti%

Cr%

Nb+Ta%

max

67.00

max

max

18.00

2.00

0.50

min

1.00

0.75

22.00

3.00

 

Tensile Strength ≥600 MPa
Yield Strength ≥360 MPa
Elongation ≥30 MPa
Impact Strength ≥100 MPa

Mechanical properties are approximate and may vary based on the heat, shielding gas, welding parameters and other factors.

 

Shielding Gases

EN ISO 14175 – I1, I3

 

Welding Positions

EN ISO 6947 – PA, PB, PC, PD, PE, PF

 

Packaging Data

Diameter

Weight

Spool

Pallet Qty

1.00 mm

1.20 mm

15 Kg

15 Kg

BS300

BS300

72

72

Liability: Whilst all reasonable efforts have been made to ensure the accuracy of the information contained, this information is subject to change without notice and can be only considered as suitable for general guidance.

 