Stainless Steel Flux Cored Wire E309LT-1 Flux-cored Welding Wire

Short Description:

E309LT-1 is most frequently used for base metals of similar composition such as AISI Types 301, 302, 304, 305 and 308. The 0.04% maximum carbon content allows for increased resistance to intergranular corrosion and also minimizes carbide precipitation.


Product Detail

Product Tags

Stainless Steel Flux Cored Wire E309LT-1

INTRODUCTION
E309LT-1 is most frequently used for base metals of similar composition such as AISI Types 301, 302, 304, 305 and 308. The 0.04% maximum carbon content allows for increased resistance to intergranular corrosion and also minimizes carbide precipitation. These wires have been developed for use with 100% CO2 or 80% Ar/20% CO2 shielding gas. The ability of operating over a wide range of current settings permits deposition rates that are nearly 4 times greater than covered electrodes and up to 50% greater than solid MIG wire. Although the cost per pound of Stainless Steel Flux-Cored wires may be more than that of coated electrodes or solid MIG wire, your cost per pound of deposited weld metal is greatly reduced because of the higher deposition efficiency and lower operational costs. The true stainless steel sheath used in manufacturing Aufhauser Flux-Cored Stainless is your guarantee of smooth performance, x-ray quality welds and a beautiful stainless steel bead appearance. Spatter is extremely low and slag is self-peeling.

APPLICATIONS
Welding similar alloys in wrought or cast forms
Welding dissimilar metals, such as: joining Type 304 to mild steel, welding the stainless steel side of Type 304 clad steels, and applying stainless steel sheet linings to carbon steel sheets
Occasionally used for welding Type 304 base metals in severe corrosion conditions
Used for first layer cladding of carbon steel if no columbium additions are required

GENERAL INFORMATION
Chemical Composition

Carbon Chromium Nickel Molybdenum Manganese Silicon Phosphorus Sulfur Copper Iron
0.04 22.0-25.0 12.0-14.0 0.5 0.5-2.5 1.0 0.04 0.03 0.5 Rem

PHYSICAL AND MECHANICAL PROPERTIES

Tensile Strength 75,000 psi
Density –
Elongation, min. % 30

 

SPECIFICATIONS MEET OR EXCEED
AWS: A5.22
ASME: SFA 5.22

 

STANDARD SIZES AND DIAMETERS
Diameters: 0.035″, 0.045″, and 1/16″

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.