Flux Cored Welding Wire, Grade: A 5.22 E308L T1-1 Stainless Steel Wire

Short Description:

For welding of Low Carbon 18-20% Cr/ 8-12% Ni steels with excellent weld ability Due to the presence of ferrite, the weld metal has lower Susceptibility to cracking. Mechanical properties are superior in as Welded condition and have better intergranular corrosion resistance due to lower carbon content.


Product Detail

Product Tags

Flux Cored Welding Wire, Grade: A 5.22 E308l T1-1

Product Specification

Wire Material SS
Quantity Per Roll 15 kg
Packaging 15 kg per pack
Grade A 5.22 E308L T1-1
Packaging Type Spool sealed in polythene bag and shrink wrapped in a corrugated box
Thickness 1.2MM 1.6MM
Current 190-300A
Wire Extension 20-25mm (stickout)
Available Size 2.00mm,2.4mm
Polarity DC wire positive
Shielding Gas CO2 gas with flow rate of 15-20 litres/minute
Weld Mechanical Properties UTS=520N/mm2 Min; Elongation(%)=35% min
Weld metal chemistry C= 0.035%,Mn=1.65%,P=0.02%,Si=0.50%,S=0.008%,Ni=9.50%,Cr=19.50%

Product Description
The stainless steel flux cored wire having stable and smooth arc, with good slag detachability

Applications:
For welding of Low Carbon 18-20% Cr/ 8-12% Ni steels with excellent weld ability Due to the presence of ferrite, the weld metal has lower Susceptibility to cracking. Mechanical properties are superior in as Welded condition and have better intergranular corrosion resistance due to lower carbon content.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.


  • Previous: