AWS A5.22 E312T-1 FLUX-CORED WIRE

Chemical Composition

Fe C Cr Ni Mo Mn Si P S N Cu
Balance 0.15 28.0-32.0 8.0-10.5 0.5 0.5-2.5 1.0 0.04 0.03 — 0.5

Single values are maximum unless otherwise specified.

Description and Applications
E312T-1 is a flux-cored AISI 312 type stainless steel alloy wire with exceptionally good operating characteristics. It produces dense, tough deposits having the highest tensile strength of any of the austenitic stainless steels. Weld deposits match the characteristics and mechanical properties of AISI 312 base metal. Weld deposits are approximately 23 Rockwell C as applied. Machining should be done with slow feed rates as the weld deposits are resistant to heat, corrosion and wear. The unique metallurgical structure is that of ferrite suspended in an austenite matrix. This makes the deposits extremely resistant to cracking.
It is used to weld base metals of similar analysis as well as dissimilar steels. Inweld E312T-1 performs well on abrasion-resisting steels, manganese steels, hardening steels, spring steels, armor plate, high-yield steels and for joining high temperature steels to carbon and low alloy steels. An excellent choice as an underlay (buffer layer) for hard-facing deposits.
Typical Weld Metal Properties
AWS Spec Tensile Strength: 95,000 psi Yield Strength: 75,000 psi
Elongation: 35%

Recommended Parameters
FCAW (DCEP – Electrode +) 100% CO2 or 75% – 95% Ar / Balance CO2

 

Wire Diameter Voltage Amperage
0.045” 25-30 130-180
1/16” 24-29 160-250

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.