AWS E70T-1 CO2 Gas-Shielded Flux Cored Welding Wire

Short Description:

AWS E70T-1 CO2 Gas-Shielded Flux Cored Welding Wire. Used for welding structures made of carbon steel and low-alloy structural steel with tensile strength higher than or equal to 490MPa.


Product Detail

Product Tags

AWS E70T-1 CO2 Gas-Shielded Flux Cored Welding Wire

Used for welding structures made of carbon steel and low-alloy structural steel with tensile strength higher than or equal to 490MPa. Most widely used for welding some key structures like shipbuilding, mechanical manufacture, pressure vessels, boilers, petroleum machinery, chemical machinery, hoisting machinery, etc.

 Size   0.8mm 1.0mm 1.2mm 1.6mm 2.0mm 2.4mm 3.0mm 3.2mm 4.0mm
  Applications Used for welding structures made of carbon steel and low-alloy structural steel with tensile strength higher than or equal to 490MPa. Most widely used for welding some key structures like shipbuilding, mechanical manufacture, pressure vessels, boilers, petroleum machinery, chemical machinery, hoisting machinery, etc.

 

Chemical composition of deposited metal(%)
C
≤0.18
Si
≤0.90
Mn
≤1.75
S
≤0.03
P
≤0.03

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.


  • Previous: