AWS E9016-B3 Heat Resistant Steel Welding Electrode R406 Wear-Resistant Welding Electrode

Short Description:

R406 (AWS E9016-B3 ) is a pearlitic heat-resistant steel electrode with a low-hydrogen potassium coating containing 2.5% Cr – 1% Mo.


Product Detail

Product Tags

Molybdenum and Chromium Molybdenum Heat Resistant Steel Welding Electrode

R406                                                         

GB/T E6016-B3

AWS A5.5 E9016-B3                      

Description: R406 is a pearlitic heat-resistant steel electrode with a low-hydrogen potassium coating containing 2.5% Cr – 1% Mo.Both AC and DC can be used, and can be welded in all positions. The weldment must be preheated to 160 ~ 200°C before welding.

Application: Used for welding Cr2.5Mo pearlitic heat-resistant steel structures, such as high-temperature and high-pressure pipelines with operating temperatures below 550 ° C, synthetic chemical machinery, and petroleum cracking equipment.

 

Chemical composition of weld metal(%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.50

2.00 ~ 2.50

0.90 ~ 1.20

≤0.030

≤0.030

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Yield strength

Mpa

Elongation

%

Impact value (J)

Normal Temp.

Guaranteed

≥590

≥490

≥15

≥47

 

Diffusion hydrogen content of deposited metal: ≤4.0mL/100g (glycerin method)

 

X-ray inspection:  I grade

 

Recommended current:

Rod diameter

(mm)

2.5

3.2

4.0

5.0

Welding Current

(A)

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Notice:

1. The electrode must be baked for 1 hour at around 350℃ before welding operation;

2. It is essential to clean up rusty, oil scale, water, and impurities on welding parts before welding.

 