AWS: E70T-6-H16, E70T6-A2-CS3-H16 Flux-cored Self-shielded (FCAW-S) Wire Flux Cored Welding Wire

Short Description:

AWS: E70T-6-H16, E70T6-A2-CS3-H16 Flux-cored self-shielded (FCAW-S) Wire.Designed for in-position, high deposition welding on carbon steel.


Product Detail

Product Tags

AWS: E70T-6-H16, E70T6-A2-CS3-H16
AWS: E70T-6-H16, E70T6-A2-CS3-H16 Flux-cored self-shielded (FCAW-S) Wire.Designed for in-position, high deposition welding on carbon steel. Recommended in single or multiple pass, automatic and semiautomatic welding.

FEATURES
High deposition rates in the flat and horizontal positions
Smooth arc and low spatter levels
Capable of producing weld deposits with impact properties exceeding 27 J (20 f:Ibf) at -29°C (-20°F)
Welds on lightly rusted or primed plate

Typical Applications
General plate fabrication
Structural fabrication, including those subject to seismic requirements
Shipyards, stiffener welding on barges
Bridges and offshore rigs
Welding over tack welds made with stick electrode

DEPOSIT COMPOSITION

Classification Polarity %Ai %B %C %Mn %P %S %SI Diffusible Hydrogen
mL/100g Weld Metal
E70T-6- H8 DC+     0.03 max. 1.75 max. 0.03 max. 0.03 max. 0.6 max. 8.0 max.
E70T6- A2-CS3-H8 DC+     0.03 max. 1.75 max. 0.03 max. 0.03 max. 0.6 max. 8 max.
Typical Result DC+ 0.7-1.0 0.0019 0.05-0.08 1.19-1.61 0.02 0.01 0.17-0.28 5.1

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.