AWS A5.22 E317LT1-1 Flux Cored Arc Welding Wire
JIS Z 3323 TS 317L-FC11
Characteristics and Application
AWS A5.22 E317LT1-1 Flux Cored Arc Welding Wire is designed for 100% CO2 gas shielding and all-position welding wire.
It is used for joining types of stainless steelssuch CF -8M and CF-3M. The weld metal exhibits excellent performance of pitting inter-granular corrosion resistance. Common applications include offshore fabrication, chemical tankers as well as petro-chemical, pulp and paper industries.
Typical chemical Composition of Weld Metal (%)
C 0.027 Mn 1.32 Si0.59 P 0.028 S 0.007 Cr 19.20 Ni 13.14 Mo 3.57
Typical Mechanical Properties of Weld Metal
Tensile Strenght 620MPa Elongation 34%
Notes on usage: .
1. Before welding, oil, rusty, and moisture should be cleaned off the base material that should have the proper
protection from the wind in welding site.
2. Use 99.8% or higher purity CO2 as shielding gas.
3. Keep the product dry, while it is stored or delivered.
Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.
Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.