Stainless Steel Welding Electrode
SIA(Rutile) is an electrode depositing 18Cr-8Ni-5Mn weld metal. Ideally suited for joining and surfacing applications to enhance resistance to impact and abrasion. Ideally suited for joining austenitic manganese steel to carbon steel, low alloy steel, etc. , and also for buffer layers on a variety of steels.
Precaution
1. Ensure the electrodes are dry. Re-dry the electrodes at 200-250 C for one hour.
2. Use short arc and minimum heat input.
CHEMICAL COMPOSITION OF ALL WELD METAL (%)
| Element | C | Mn | Si | Cr | Ni |
| Percent | 0.07 | 6.0 | 0.60 | 19.0 | 9.0 |
MECHANICAL PROPERTIES OF ALL WELD METAL
| UTS | Elongation | Hardness |
| (MPa) | (L= 4d)% | 200-220 BHN (As welded) |
| 614 | 35.0 | 500 BHN (Work hardens under impact) |
CURRENT AND PACKING DATA: AC / DC(+)
|
Size (mm) |
5x350 |
4x350 |
3.15x350 |
2.5x350 |
|
Current Range (Amps) |
190-240 |
140-190 |
90-130 |
60-100 |
|
Qty. (Pcs./Carton) |
25 |
40 |
60 |
80 |
Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.
Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.