AWS E10015-G (J707Ni) Low Alloy Steel Welding Electrode Welding Stick

Short Description:

J707Ni (AWS E10015-G) is a low-alloy high-strength steel electrode with low-hydrogen sodium coating.


Product Detail

Product Tags

Low Alloy Steel Welding Electrode

J707Ni                                   

GB/T E7015-G

AWS E10015-G                     

 

Description: J707Ni is a low-alloy high-strength steel electrode with low-hydrogen sodium coating. Use DCEP (direct current electrode positive) and can be welded in all positions. Deposited metal has good mechanical properties. Compared with J707 electrode, the main feature of J707Ni is that the low temperature toughness and crack resistance have been significantly improved.

Application: Used for welding low-alloy high-strength steel structures of corresponding strength levels, such as 14MnMoVB, WEL-TEN70 and Japanese HW56 and other low-alloy high-strength steel structures.

 

Chemical composition of weld metal(%):

C

Si

Mn

Ni

Mo

Cr

S

P

≤0.10

≤0.60

≥1.00

1.80 ~ 2.20

0.40 ~ 0.60

≤0.20

≤0.030

≤0.030

 

 Mechanical properties of weld metal:

 

Test item

 

Tensile strength

Mpa

 

Yield strength

Mpa

 

Elongation

%

 

Impact value (J)

-40℃

-50℃

 

Guaranteed

≥690

≥590

≥15

—

≥27

 

Tested

760

630

23

140

—

 

 

Diffusion hydrogen content of deposited metal: ≤4.0mL/100g (glycerin method) 

 I级      X-ray inspection:  I grade

 

 Recommended current:

       (mm)

Rod diameter

2.5

3.2

4.0

5.0

(A)

Welding Current

60 ~ 100

100 ~ 140

140 ~ 190

190 ~ 250

 

 

Notice:

1. The electrode must be baked for 1 hour at 350 ~380℃ before welding operation;

2. It is essential to clean up rusty, oil scale, water, and impurities on welding parts before welding;

3. Use short arc operation when welding. The narrow welding track is proper.

 