Low Alloy Steel Welding Electrode AWS E7018-G Welding Rods Iron Power and Low Hydrogen

Short Description:

J507FeNi (AWS E7018-G)  is a low alloy steel electrode with iron powder and low hydrogen coating. It can be used for all-position welding with AC and DC


Product Detail

Product Tags

Low Alloy Steel Welding Electrode

J507FeNi                                                        

GB/T E5018-G  

AWS E7018-G                                 

Description: J507FeNi is a low alloy steel electrode with iron powder and low hydrogen coating. It can be used for all-position welding with AC and DC. The performance stability of AC welding is inferior to that of DC welding

Application: Used for welding medium carbon steel and low temperature steel pressure vessels, such as 16MnDR, etc.

Chemical composition of weld metal(%):

C

Mn

Si

Ni

S

P

≤0.08

0.80 ~ 1.30

≤0.65

1.20 ~ 2.00

≤0.030

≤0.030

 

Mechanical properties of weld metal:

Test item

 

Tensile strength

Mpa

 

Yield strength

Mpa

 

Elongation

%

 

Impact value (J)

-40℃

Guaranteed

≥490

≥390

≥22

≥54

 

Diffusion hydrogen content of deposited metal: ≤6.0mL/100g (glycerin method)

X-ray inspection:  I grade

 

Recommended current:

Rod diameter
(mm)

3.2

4.0

5.0

Welding Current

(A)

90 ~ 120

140 ~ 180

170 ~ 210

 

Notice:

1. The electrode must be baked for 1 hour at about 350℃ before welding operation;

2. It is essential to clean up rusty, oil scale, water, and impurities on welding parts before welding.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 