Classifications:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Characteristics:

AWS A5.1 E6013 (J421X) is a rutile type electrode. Can be welding both AC & DC power source and can be for all position. It have excellent welding performance as stable arc, little spatter, easy slag removal and reignition-ability etc. Rutile-cellulosic electrode with good weld ability in all positions including vertical down. Excellent gap-bridging and arc-striking ability. For tack welding and load fit ups. General purpose for industry and trade, assembly and shop welding.

Chemical Composition of All Weld Metal: (%)
Chemical Composition C Mn Si S P Ni Cr Mo V
Requirements ≤0.10 0.32-0.55 ≤0.30 ≤0.030 ≤0.035 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Typical Results 0.08 0.37 0.18 0.020 0.025 0.030 0.035 0.005 0.004
Mechanical Properties of Deposited Metal
Test Item Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Requirements 440-560 ≥355 ≥22 ≥47
Typical Results 500 430 27 80
Reference Current (DC)
Diameter φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 80 ~ 130 150 ~ 210 180 ~ 240

Welding Position:

PA, PB, PC, PD, PE, PF

X-Ray Radiographic Inspection:

Level Ⅱ

Attention: