AWS E7015 Welding Rods

Short Description:

AWS A5.1 E7015 is low-hydrogen sodium coated carbon steel electrode.


Product Detail

Product Tags

AWS A5.1 E7015 is low-hydrogen sodium coated carbon steel electrode.

E7015 welding electrode must be operated on DCEP. It has very good welding usability that enables it to perform all-position welding, has stable arc, removal of slag is easy and has low spatter. The deposited metal has good mechanical performance and crack-resistance, which offers good low temperature toughness.

Application

AWS A5.1 E7015 is applied in welding medium-carbon steel and low-alloy structures such as 16Mn, 09Mn2Si, 09Mn2V and the steels used in shipbuilding such as A, B, D, E. It is also used in thick steel plates and the carbon steel structures that are difficult to weld.

Conform to Standard

GB/T 5117 E5015

AWS A5.1 E7015

ISO 2560-B-E 49 15 A

Purpose:AWS A5.1 E7015 is applied in welding medium-carbon steel and low-alloy structures such as 16Mn, 09Mn2Si, 09Mn2V and the steels used in shipbuilding such as A, B, D, E. It is also used in thick steel plates and the carbon steel structures that are difficult to weld.

Chemical Composition(%)

Chemical Composition

C

Mn

Si

S

P

Ni

Cr

Mo

V

Guarantee Value

≤

0.15

≤

1.60

≤

0.90

≤0.035

≤0.035

≤

0.30

≤

0.20

≤

0.30

≤

0.08

General Result

0.082

1.10

0.58

0.012

0.021

0.011

0.028

0.007

0.016

Mechanical Properties of Deposited Metal(Shielding Gas:CO2)

Test Item

Rm(MPa)

ReL(MPa)

A(%)

KV2(J)

-20℃ -30℃

Guarantee Value

≥490

≥400

≥20

≥47

≥27

General Result

550

450

32

150

142

X-Ray Radio-graphic Test Requirements:Grade I

Reference Current(DC+)

Diameter(mm)

Φ2.5

Φ3.2

Φ4.0

Φ5.0

Amperage(A)

60~100

80~140

110~210

160~230

Notes:

1. The electrode must be preheated at the temperature of 350°C for 1 hour. Preheat the rod whenever it is used.

2. The impurities such as rust, oil stains and moisture must be cleared off of the work piece.

3. Short arc is required to perform welding. Narrow weld path is preferred.


  • Previous: