AWS E6010 Mild Steel Welding Electrode, Carbon Steel Welding Rods, High Cellulose Welding Stick

Short Description:

J425G (AWS E6010) is a high cellulose sodium-coated vertical downward electrode.


Product Detail

Product Tags

Carbon Steel Welding Electrode 

J425G                                                         

GB/T E4310

AWS A5.1 E6010                                    

Description: J425G is a high cellulose sodium-coated vertical downward electrode. Use DCEP (direct current electrode positive), which is suitable for all-position vertical downward welding of the circular seam on the pipeline site. When welding the bottom layer, it can be welded on one side and formed on both sides, and the welding speed is fast.

Application: Used for circumferential seam welding of various carbon steel pipes.

 

Chemical composition of weld metal(%):

C

Mn

Si

S

P

≤0.20   

0.30~0.60

≤0.20

≤0.035

≤0.040

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Yield strength

Mpa

Elongation

%

Impact value (J)

(-30℃)

Guaranteed

≥420

≥330

22

≥27

 

X-ray inspection:  II grade

 

Recommended current:

Rod diameter

(mm)

2.5

3.2

4.0

5.0

Welding current

(A)

40 ~ 70

70 ~ 110

110 ~ 160

160 ~ 190

 

Notice:

1. Unpack the welding rod before use, and use it up as much as possible after unpacking;

2. Generally, there is no need to dry it again before welding, and it can be dried at 70~90°C for 1 hour when it is damp.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 