AWS E317L-16 Stainless Steel Welding Electrode, Welding Stick for Manual Metal Arc Welding

Short Description:

A032Mo (AWS E317L-16) is an ultra-low carbon Cr19Ni13Mo3 stainless steel electrode with titanium calcium coating.


Product Detail

Product Tags

Stainless Steel Welding Electrode

A032Mo                                            

GB/T E317L-16

AWS E317L-16                

Description: A032Mo is an ultra-low carbon Cr19Ni13Mo3 stainless steel electrode with titanium calcium coating. It can be used for both AC and DC with good process performance. The corrosion resistance to sulfuric acid, sulfurous acid and organic acid is better than that of E316L.

Application: It is used for welding the same type of stainless steel materials such as AISI317 and 317L steel, and is also suitable for welding and surfacing corrosion-resistant layers of composite steel and special-shaped steel.

 

Chemical composition of weld metal(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

3.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Elongation

%

Guaranteed

≥520

≥25

 

Recommended current:

Rod diameter

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 220

 

Notice:

1. The electrode must be baked for 1 hour at around 250℃ before welding operation;

2. It is essential to clean up rusty, oil scale, water, and impurities on welding parts before welding.

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.