AWS A5.1 E7018-1 H4
EN ISO 2560-A-E 46 4 B 12 H5
JIS Z 3211 E4918-1 H5
Characteristics and Application
AWS A5.1 E7018-1 H4 Welding rods, welding electrode is an iron-powder low hydrogen type electrode for all-position welding of 490N/mm2 grade high tensile steel. It is designed for single and multiple pass applications. The product has good welder appeal and produces a stable arc with low spatter generation. it produces weld metals with excellent mechanical properties and impact toughness at low temperature (-45℃) and low diffusible hydrogen. Its features make the product suitable for low alloy steels, medium carbon steels, heavy steel plates, cast steels, aluminum killed steel of LPG and especially for welding of steels with poor weldability.
Typical chemical Composition of Weld Metal (%)
| C | Mn | Si | P | S |
| 0.065 | 1.40 | 0.60 | 0.020 | 0.070 |
Typical Mechanical Properties of Weld Metal
| Yield strength | Tensile strength | Elongation | Charpy V-Notch(-45℃) |
| 520Mpa | 620Mpa | 32% | 120J |