E7018 carbon steel welding rod

Short Description:

Welding Rods AWS E7018 is a low hydrogen iron potassium powder coated carbon steel electrode.


Product Detail

Product Tags

Classification:

AWS A5.1 E7018

ISO 2560-B-E4918A

GB/T 5117 E5018

Welding Rods AWS E7018 is a low hydrogen iron potassium powder coated carbon steel electrode. Iron dust in the coating increases the deposit rate. It has very good usability that allows it to have a stable arc, little spatter, slag removal is easy and welds in all positions. The deposited metal has good mechanical properties offering very good low temperature toughness.

AWS E7018 welding rod (basic iron powder type electrode) is suitable for the welding of carbon steel and low alloy steel structure, such as Gr.50, and so on.

Chemical composition (%)
Chemical Composition

C

Mn

Si

S

P

Guarantee Value

≤0.12

≤1.60

≤0.75

≤0.035

≤0.040

General Result

0.089

1.2

0.38

0.028

0.04

Mechanical properties of deposited metal
Test Item

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) -30°C

Guarantee Value

≥490

≥400

≥20

≥27

General Result

515

430

32

156

Reference current (DC)

Diameter

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

60 ~ 100

80 ~ 140

110 ~ 210

160 ~ 230

X-ray Radiographic Inspection: Grade Ⅰ

Welding Position:

PA, PB, PC, PD, PE, PF

Notes:
1. The electrode must be preheated at the temperature of 350°C for 1 hour. Preheat the rod whenever it is used.
2. The impurities such as rust, oil stains and moisture must be cleared off of the work piece.
3. Short arc is required to perform welding. Narrow weld path is preferred.