Hardfacing Welding Electrode DIN 8555 (E10-UM-65-GRZ) Surfacing Welding Rod Type No.: TY-C LEDURIT 67 Arc Welding Stick

Short Description:

DIN 8555 (E10-UM-65-GRZ) is  a  basic coated high recovery SMAW electrode for hardsurfacing.


Product Detail

Product Tags

Hardfacing Welding Electrode

 

Standard: DIN 8555 (E10-UM-65-GRZ)

Type No.: TY-C LEDURIT 67

 

Specification & Application:

· Basic coated high recovery SMAW electrode for hardsurfacing.

· Extra hard surfacing of parts undergoing heavy abrasion and moderate impact.

· Suitable for final hard layers after buffer layer.

· Sinter plant parts, wear bars and plates, scraper bars, blast furace, charging systems, cement furnaces, bucket teeth and lips, screens.

 

Chemical composition of deposited metal(%):      

 

C

Si

Mn

Cr

B

DIN

High C content and Cr content

Typical

3.5

1.0

1.8

35

1.0

 

Hardness of deposited metal:

Pure weld deposit

(HRC)

1 layer on 0.15% steel

(HRC)

2 layer on 0.15% steel

(HRC)

62 – 65

59 – 63

61 – 64

 

General Characteristics:   

· Microstructure      Martensitic+Austenite+Carbides

· Machinability       Grinding only

· Redrying           Redry for 2 h at 300℃ before using.