B-85 Hardfacing Welding Electrode, Surfacing Welding Rod, Arc Welding Stick

Short Description:

The coating of this electrode has a high chromium content, which makes its deposit very resistant to wear due to extreme abrasion, severe friction and low impact, even at high temperatures and in corrosive atmospheres. It should not be exposed to severe shock or impact.


Product Detail

Product Tags

Hardfacing Welding Stick Electrode

 RECUBRIMIENTO PROTECTOR

Type No.: B – 85

Deposited Metal Analysis (Typical values)

C

4.0%

Si

0.6%

Cr

35%

 

Characteristics:

The coating of this electrode has a high chromium content, which makes its deposit very resistant to wear due to extreme abrasion, severe friction and low impact, even at high temperatures and in corrosive atmospheres. It should not be exposed to severe shock or impact.

 

Mechanical Properties: Hardness from 57 to 62 HRc. (Two covers)

 

Current and Polarity:

Preferable alternating current in direct current, electrode to the positive pole

ø mm.

1/8”

5/32”

3/16”

Amp. min.

120

170

220

Amp. max.

140

190

250

 

Applications:

• Coat screw conveyors

• Excavator buckets

• Scarifier teeth

• Dredge pumps

• Mining machinery

• Sand pumps

 

 

LENGTH: 350mm.

WEIGHT PER BOX: 20 kg/44 lbs.

 

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 

 