TYUE E308-16 STAINLESS STEEL ELECTRODE

Short Description:

Line titanium type welding electrode for extra-low carbon stainless steel.


Product Detail

Product Tags

Classification:

AWS A5.4 / ASME SFA5.4 E308-16

JIS Z3221 D308-16

Description :

Stainless Steel Welding Electrode E308-16 is a line titanium type welding electrode for extra-low carbon stainless steel.The weld metal has excellent mechanical properties and shows good resistance to intergranular corrosion due to the carbon content in it is ≤. 0.04% b. It can be used for all position welding with excellent performance:stable arc,small spatters,good appearance of weld.And also the welding electrode shows good heat-resistance character,not easy to turn red and gas porosity is not produced.

Application :

Welding of 18%Cr-8%Ni steel.

It is suitable for welding structures fabricated by extra-low carbon 022Cr-19Ni10 stainless steel,such as synthetic fibre,fertilizer,

petrochemical equipment, etc.

Chemical Composition of Deposited Metal(E308L-16) (%)

 Item C Mn Si Cr Ni S P Cu Mo
standard value ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
Example value 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

Mechanical Properties of Deposited Metal (%)

The anti-corrosion performance and ferrite composition should be detemined between buyer and seller.

Item Tensile  Strength(MPa) Elongation  (%)
standard value ≥550 ≥25
Example value 601 41

Diameter(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current (A)

25-50

50-80

80-110

110-160

160-200

 

Notes on Usage:

1.Keep the arc as short as possible.

2.Remove dirts such as oil and dust from the groove.

3.Dry the electrodes at 350 (662 ) for 60 minutes before use