ZELLER D350(UTP DUR 350) WEAR RESISTANCE ELECTRODE

Short Description:

UTP DUR 350 is particularly suited for wear resistant surfacings on MnCrV alloyed parts.

Product Detail

Product Tags

Classifications
DIN 8555/EN 14700
E1-UM-350/E Fe1
Characteristics and field of use
UTP DUR 350 is particularly suited for wear resistant surfacings on MnCrV alloyed parts, such as
frogs, track rollers, chain support rolls, sprocket wheels, guide rolls etc. The deposit is still
machinable with tungsten carbide tools.
UTP DUR 350 has a very good resistance against compression and rolling strain in combination
with slight abrasion. The weld metal is machinable with tungsten carbide tools.
Hardness of the pure weld deposit    approx. 370 HB
1 layer on steel with C = 0.5 %            approx. 420 HB
Typical analysis in %
C Si Mn Cr Fe
0.2 1.2 1.4 1.8 Balance