E6010 carbon steel welding electrode

Short Description:

E6010 is a rutile-cellulosic sodium type electrode.


Product Detail

Product Tags

AWS E6010 Mild Steel Welding Electrode

APPLICATIONS:

It is suitable for welding of low carbon steel structure as pipeline, shipbuilding and bridge etc.

CLASSIFICATIONS:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

CHARACTERISTICS:

E6010 is a rutile-cellulosic sodium type electrode. Can be weld for all-position (especially for vertical-down position) with DC+ only. It have excellent welding performance as stable arc, little spatter, easy slag removal and reignition-ability etc. Better molten pool control, stronger arc force and deeper penetration at vertical-down position.

CHEMICAL COMPOSITION OF ALL WELDS METAL: (WT. %)

Items C Mn Si S P Ni Cr Mo V
Requirements ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Typical Results 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

MECHANICAL PROPERTIES OF ALL WELD METAL:

Items Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃) /J
Requirements ≥430 ≥330 ≥20  ≥27
Typical Results 475 400 26 80

ATTENTION:

1. In generally, don’t need to re-dry the electrode before welding. When it be affected with damp, should be re-dry it at 70℃-90℃ for 1 hour.

2. The rust, oil, water and other impurities of the weld area must be removed before welding.

TYPICAL OPERATING PROCEDURES: ( DC+)

Diameter (mm) 2.5 3.2 4.0 5.0
Length (mm) 300 350 400 400
Current (A) 50-80 60-100 100-140 140-180

PACKAGING:

5kg/box, 4boxes/carton, 20kgs/carton, 50cartons/pallet. 21MT -26MT per 1X20″ FCL.

 

OEM/ODM:

We support OEM/ODM and could make packaging according to your design, please contact us for detail discussion.

 

Characteristics on Usage:

Very stable arc.

Excellent removability of slag.

Penetration is shallow.

Good heat and corrosion resistance.

Excellent crack resistance.


  • Previous: