AWS E6013 (J421) Carbon Steel Welding Electrode Rutile Welding Rods

Short Description:

J421 (AWS E6013) is a carbon steel electrode with high titanium and potassium coating. It can be used for all-position welding with AC and DC.


Product Detail

Product Tags

Carbon Steel Welding Electrode

 J421                                                         

GB/T E4313

AWS A5.1 E6013                                    

Description: J421 is a carbon steel electrode with high titanium and potassium coating. It can be used for all-position welding with AC and DC. It has high welding performance and is easy to restart the arc.

Application: Suitable for welding low carbon steel structures, especially suitable for intermittent welding of small pieces of thin plates and short welds and cover welding requiring smooth surfaces.

 

Chemical composition of weld metal(%):

C

Mn

Si

S

P

≤0. 12

0.30~0.60

≤0.30  

≤0.035

≤0.040

 

Mechanical properties of weld metal:

Test item

Tensile strength

Mpa

Yield strength

Mpa

Elongation

%

Impact value (J)

Normal Temp.

 0℃

Guaranteed

≥420

≥330

≥17

—

—

Tested

460 ~ 540

≥340

18 ~ 26

50 ~ 75

≥47

  X-ray inspection:  II grade

Recommended current:

Rod diameter

(mm)

2.0

2.5

3.2

4.0

5.0

5.8

Welding current

(A)

40 ~ 70

50 ~ 80

80 ~ 120

150 ~ 190

180 ~ 240

220 ~ 280

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 