AWS E6011 welding electrode is type of cellulose potassium, which is used for vertical down welding. Both for AC and DC welding.


Product Detail

Product Tags

Application
Welding rods AWS E6011 it is suitable for welding vessel structures such as buildings and bridges, storages tanks, pipes and pressure vessel fittings.

AWS E6011 welding electrode is type of cellulose potassium, which is used for vertical down welding. Both for AC and DC welding. It adopts advanced foreign technology and has excellent welding technological properties. The length of ARC should be controlled in a reasonable range. It is not proper multilayers welding and cover welding.

Chemical Composition (%)
C Mn Si S P
≤0.2 0.3-0.6 ≤0.22 ≤0.03 ≤0.04
Mechanical Properties of Deposited Metal
Test Item Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Guarantee Value ≥420 ≥330 ≥22 ≥47
General Result 485 380 24 86
Reference Current (DC)
Diameter φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

TYPE OF CURRENT: Direct Current Electrode Positive (DCEP) or AC

RECOMMENDED WELDING TECHNIQUES:

Arc Length – Average length (1/8” to 1/4”)

Flat – Stay ahead of puddle and use slight whipping motion

Horizontal – Angle electrode slightly toward top plate

Vertical Up – Slight whipping or weaving technique

Vertical Down – Use higher amperage and faster travel, staying ahead of puddle

Overhead – Stay ahead of puddle and use slight whipping motion

Attention:
1. It is easy to expose to moisture, please keep it in dry condition.
2. It needs heating when package breaks or moisture absorbed, heating temperature should be between 70C to 80C, heating time should be from 0.5 to 1 hour.
3. When using 5.0mm welding electrodes, it’s better to use high-thrust, low-current, in order to enhance welding performance.