ER5356 Aluminum Welding Wire Welding Rods and Electrodes

Short Description:

ER5356   is a general-purpose type aluminum alloy which is typically chosen for its relatively high shear strength.


Product Detail

Product Tags

ER5356   is a general-purpose type aluminum alloy which is typically chosen for its relatively high shear strength.  In addition, it also offers excellent corrosion resistance when exposed to salt water.  ER5356 should be considered for welding 5000 series aluminum base metals.

Typical Applications:  welding filler wire

AWS Class: ER5356 Certification:  AWS A5.10/ A5.10M:1999
Alloy:  ER5356 AWS/ASME SFA A5.10
Welding Position:
F, V, OH, H
Current:
DCEP-GMAW
AC-GTAW
Typical Properties (as welded)
Conductivity: 29% IACS (-0)/27% IACS (-H18)
Tensile Strength, kpsi: 38
Color: White
Melting Point 1175⁰F Solidification 1060⁰F Density 0.096 lbs/cu In.
Typical Wire Chemistry as per AWS A5.10 (single values are maximum)
Si Fe Cu Mn Mg Cr Zn Ti Other AL
0.25 0.40 0.10 0.50-1.0 4.7-5.5 0.05-0.20 0.25 0.05-0.20 0.15 Remainder
Typical Welding Parameters
Diameter Process Volt Amps GAS
in (mm)
.030  (.8) GMAW 15-24 60-175 Argon (cfh)
.035  (.9) GMAW 15-27 70-185 Argon (cfh)
3/64” (1.2 ) GMAW 20-29 125-260 Argon (cfh)
1/16” (1.6) GMAW 24-30 170-300 Argon (cfh)
3/32” (2.4) GMAW 26-31 275-400 Argon (cfh)
Diameter Process Volt Amps GAS
in (mm)
 1/16”  (1.6) GTAW 15 60-80 Argon (cfh)
 3/32”  (2.4) GTAW 15 125-160 Argon (cfh)
 1/8”  (3.2) GTAW 15 190-220 Argon (cfh)
5/32”  (4.0 ) GTAW 15 200-300 Argon (cfh)
3/16” (4.8) GTAW 15-20 330-380 Argon (cfh)

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 