Hardfacing Welding Electrode Surfacing Welding Rods DIN 8555 (E10-UM-60-GRZ) Stick Electrode for Arc Welding

Short Description:

DIN 8555 (E10-UM-60-GRZ) is a basic coated high recovery SMAW electrode for hardsurfacing.


Product Detail

Product Tags

Hardfacing Welding Electrode

 

Standard: DIN 8555 (E10-UM-60-GRZ)

Type No.: TY-C LEDURIT 61

 

Specification & Application:

· Basic coated high recovery SMAW electrode for hardsurfacing.

· Extra hard surfacing of parts undergoing heavy abrasion and moderate impact.

· Suitable for final hard layers after buffer layer.

· Sinter plant parts, wear bars and plates, scraper bars, blast furace, charging systems, cement furnaces, bucket teeth and lips, screens.

 

Chemical composition of deposited metal(%):      

 

C

Si

Mn

Cr

Mo

Nb

W

V

Ni

Fe

DIN

High C content and Cr content

Bal.

EN

1.5

4.5

-

0.5

3.0

25

40

-

4.0

-

-

-

-

4.0

Bal.

Typical

3.2

1.0

1.8

29

-

-

-

-

-

Bal.

 

 

Hardness of deposited metal:

As Welded

(HRC)

1 layer on steel with C=0.15%

(HRC)

1 layer on high Mn-steel

(HRC)

60

55

52

 

General Characteristics:   

· Microstructure      Martensitic+Austenite+Carbides

· Machinability       Grinding only

· Redrying           Redry for 2 h at 300℃ before using.

 