AWS ERCU Copper Alloy Welding Wire Brass Welding Wire

Short Description:

ERCu is a deoxidized copper alloy developed to provide dense, high-quality deposits with relatively high electrical conductivity for use in joining and overlay with the inert-gas processes.


Product Detail

Product Tags

ERCu is a deoxidized copper alloy developed to provide dense, high-quality deposits with relatively high electrical conductivity for use in joining and overlay with the inert-gas processes.
ERCu spooled wire and filler metal rod are used primarily to fabricate deoxidized copper and repair weld copper castings with the gas metal-arc and gas tungsten-arc processes. It may also be used to weld galvanized steel and deoxidized copper to mild steel where high strength joints are not required.
ERCu spooled wire and filler metal rod are used to overlay surfaces to resist corrosion. ERCu is typically used for billet molds, conductor rolls, heater elements, copper sculptures, steel mill electrode holders, bus bars, and copper connectors.

Physical performance and mechanical properties:
Solid-phase 1020 DEG C density 8.9kg/dm Extension rate of 30-40%
liquidus 1050 DEG C tensile strength 210-220N/mm2, Brinell hardness 60HB

ERCU COPPER ALLOY WELDING WIRE CHEMICAL COMPOSITE

Chemical Composite (%)
Standards ISO 24373 GB/T9460 BS EN14640 AWS A5.7 DIN1733
Class NO. Cu1898 SCu1898 Cu1898 C18980 2.1006
Alloy NO. CuSn1 CuSn1 CuSn1 ERCu SG-CuSn
Cu Min 98 Min98 Bal. Min 98 Bal.
Al 0.01 Max 0.01 0.01 0.01 Max 0.01
Fe – – 0.05 0.50 Max 0.05
Mn 0.50 Max 0.5 0.1~0.5 0.50 0.1~0.5
Ni – – 0.3 – Max 0.3
P 0.15 Max 0.15 0.02 0.15 Max 0.02
Pb 0.02 Max 0.02 0.02 0.02 Max 0.01
Si 0.5 Max 0.5 0.5 0.5 0.1~0.5
Sn 1.0 Max 1.0 0.5~1.0 1.0 0.5~1.0
As – – 0.05 – Max 0.05
Other Total 0.5 Max 0.5 0.1 0.5 Max 0.1

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 

 