RBCuZn-A Naval Bronze (RBCuZn-A) is a copper-zinc brazing filler metal containing small amounts of tin to improve strength and corrosion resistance in the weld deposit.  It is a good choice when the high strength properties of low fuming bronze are not required.  A borax-boric acid flux is generally required when brazing with this product.

AWS Class: RBCuZn-A Certification:                  AWS A5.8/A5.8M:2011
Alloy:  RBCuZn-A ASME SFA A5.8

 

Brazing Position:              H, V Brazing Range:
1330-1550⁰F

 

Tensile Strength, kpsi: 50
Elongation %, min: 30

 

Melting Point 1650⁰F Solidification 1610⁰F Brinell Hardness 70-90

Typical Wire Chemistry as per AWS A5.8 (single values are maximum)

Cu Zn Sn Pb Al Other
57.0-61.0 Rem 0.25-1.00 0.05 0.01 0.50

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 

 