RBCuZn-B (Nickel Bronze) Brazing Filler Metals Welding Wire

Short Description:

RBCuZn-B  Nickel Bronze (RBCuZn-B) brazing filler metal is similar to naval bronze but contains manganese and iron which increase the hardness and strength of the weld deposit.


Product Detail

Product Tags

RBCuZn-B  Nickel Bronze (RBCuZn-B) brazing filler metal is similar to naval bronze but contains manganese and iron which increase the hardness and strength of the weld deposit.  It also contains nickel ensuring uniform distribution of the iron in the deposit.  A neutral or slightly oxidizing flame and a boric acid/boric type flux should be used.

AWS Class: RBCuZn-B Certification:                  AWS A5.8/A5.8M:2011
Alloy:  RBCuZn-B ASME SFA A5.8

 

Brazing Position:              H, V Brazing Range:
1620-1800⁰F

 

Tensile Strength, kpsi: 60-78
Elongation %, min: 25

 

Melting Point 1620⁰F Solidification 1590⁰F Brinell Hardness 80-110

Typical Wire Chemistry as per AWS A5.8 (single values are maximum)

Cu Zn Sn Fe Mn Ni Pb Al Si Other
56.0-60.0 Rem 0.80-1.10 0.25-1.20 0.01-0.50 0.20-0.80 0.05 0.01 0.04-0.20 0.50

 

Wenzhou Tianyu Electronic Co., Ltd. was established in 2000. We have been engaged in the manufacturing of welding electrodes, welding rods, and welding consumables for more than 20 years.

Our main products include stainless steel welding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminum welding wires, submerged arc welding. wires, nickel & cobalt alloy welding wires, brass welding wires, TIG & MIG welding wires, tungsten electrodes, carbon gouging electrodes, and other welding accessories & consumables.

 

 

 

 