    AWS:SFA 5.4 E308-16 Stainless Steel Welding Electrode

    E308-16 is a line titanium type welding electrode for extra-low carbon stainless steel.

    Classification:

    AWS A5.4 / ASME SFA5.4 E308-16

    JIS Z3221 D308-16

    Description :

    Stainless Steel Welding Electrode E308-16 is a line titanium type welding electrode for extra-low carbon stainless steel.The weld metal has excellent mechanical properties and shows good resistance to intergranular corrosion due to the carbon content in it is ≤. 0.04% b. It can be used for all position welding with excellent performance:stable arc,small spatters,good appearance of weld.And also the welding electrode shows good heat-resistance character,not easy to turn red and gas porosity is not produced.

    Application :

    Welding of 18%Cr-8%Ni steel.

    It is suitable for welding structures fabricated by extra-low carbon 022Cr-19Ni10 stainless steel,such as synthetic fibre,fertilizer,

    petrochemical equipment, etc.

     

    Chemical Composition of Deposited Metal(E308L-16) (%)

     Item C Mn Si Cr Ni S P Cu Mo
    standard value ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
    Example value 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

    Mechanical Properties of Deposited Metal (%)

    The anti-corrosion performance and ferrite composition should be detemined between buyer and seller.

    Item Tensile  Strength(MPa) Elongation  (%)
    standard value ≥550 ≥25
    Example value 601 41

    Applications

    Be used to weld the same type of heat resisting stainless steels structures working in high temperature, can also be used to weld big sclerosing chrome steel (such as Cr15Mo, Cr9Mo, Cr13, Cr28) and dissimilar steel.

    Diameter(mm)

    2.0

    2.5

    3.2

    4.0

    5.0

    Welding Current (A)

    25-50

    50-80

    80-110

    110-160

    160-200

    Current: AC or DC+

    Notes on Usage:

    1.Keep the arc as short as possible.

    2.Remove dirts such as oil and dust from the groove.

    3.Dry the electrodes at 350 (662 ) for 60 minutes before use

     