AWS: SFA 5.5 E9015-B3 Electrodes for Creep Resisting Steels

Low hydrogen electrode depositing 2.25Cr – 1Mo weld metal, display remarkable o strength and creep resistance at elevated temperatures up to 575 C. It is used for welding 21⁄4 Cr-1 Mo creep resistant steel and Cr-Mo-V steels resistant to hydrogen under pressure as well as for cast steels of a similar composition to the weld metal. Typical applications include steam boiler construction, welding of steam and super- heater piping, power plants, oil refinery and chemical plants.

CHEMICAL COMPOSITION OF ALL WELD METAL (%)

Element C Mn Si P S Cr Mo
Percent 0.05-0.12 0.5-0.9 ≤0.5 ≤0.030 0.022 2.0-2.5 0.9-1.2

MECHANICAL PROPERTIES OF ALL WELD METAL

(PWHT : 690°C FOR 1 HR)

UTS YS Elongation
(MPa) (MPa) (L= 4d)%
≥590 550 ≥15

CURRENT AND PACKING DATA: DC (+)

Size (mm)

5×450

4×450

3.15×450

2.5×350

Current Range (Amps)

200-250

150-190

100-140

70-100

Qty. (Pcs./Carton)

35

55

75

100

Precaution

1. Re-dry the electrodes at 250-300 C for one hour, as per our standard recommended practice.

2. Use short arc and stringer bead.